Porosity in Welding

welding porosity

Introduction Welding is a critical process in metal fabrication, joining materials to create sturdy and reliable structures. However, like any manufacturing process, welding is not without its challenges. One of the persistent issues faced by welders is porosity. Understanding porosity in welding is crucial for ensuring the quality and integrity …